CVD Single Crystal Diamond Plate
CVD diamond like natural diamond, has smaller friction coefficient, less cutting force and function consumption, less friction heat and excellent chip lump resistance during cutting.
The thermal conductivity of diamond is the highest among all materials, with a thermal conductivity of 1000-2000w/m.k. The thermal conductivity efficiency of thick film CVD diamond material is 5 times that of tungsten carbide, which is 50% higher than that of PCD. It can be used as a safe way to dissipate heat in the cutting area.
Nitrogen content |
50-100 ppm |
Microhardness |
80~150GPa |
Young's modulus |
1150~1300 GPa |
Thermal conductivity |
1000~2000w/m.k |
Product size |
3*3mm; 10*10mm, etc; Customizable |
Surface roughness |
Ra ≤ 10nm |